Linien

 

25 lines connected in parallel, etched into a 40 nm thick (Ga,Mn)As-channel. The linewidth is 40 nm
at a length of 7,5 mm. In this structure we have observed for the first time weak antilocalization in a ferromagnet.
Daniel Neumaier